Twelve years of battlefield experience, still sharp as ever
Release time:2019-11-06

Many people have concerns when purchasing HongboAPVCanti-corrosion tiles: Will the tiles truly last as the merchants claim,15years or even20years later, maintaining their quality?
Recently, in the Hongbo workshop, due to theCtype steel purlins corroding and falling off, they needed to be dismantled and replaced.2019year10month4day, after12years of wind, rain, and sun exposure, the HongboAPVCanti-corrosion corrugated tiles were also dismantled. What was the condition of the dismantled tiles?

The dismantled corrodedCsteel purlins

Workshop roof project completion time
(2007year2month11day)
01
12 years of APVC anti-corrosion corrugated tiles in use

Status after dismantling
APVCRinsing process

Status after rinsing

Use12years of HongboAPVCAfter rinsing, the anti-corrosion tiles still have vibrant colors, and even when a person repeatedly steps on them, there is no breakage.
02
Strength test
HongboAPVCanti-corrosion tiles2007years ago, it still used2layer co-extrusion technology processing. After testing by the engineering center, the twelve-year-old HongboAPVCanti-corrosion tile measured data is as follows:
Test1kilogram steel ball from1.5meter high free fall
Test use12yearAPVCanti-corrosion tile tensile strengthand elongation at break


Test result analysis:
(1)12After years of outdoor use, the average wear of the surface weather-resistant layer is0.121mm,that is, approximately0.01mmper year. HongboAPVCanti-corrosion tile surface layer design thickness≥0.25mm,the warranty period is20years, according to this deduction20years later, the surface wear is0.2mm,there is still a sufficient safety factor.
(2) Tensile strength: Increased by4.68%,which is a normal phenomenon. Because the product hardens after outdoor use, the tensile strength increases instead.
(3) Elongation at break: The elongation at break decreases after outdoor use, which is a normal phenomenon. After the test, the elongation loss is42%,that is, the average annual loss is3.5%,according to this deduction20years later, the elongation loss is70%,there is still a sufficient safety factor.
(4) Drop ball impact:1kgball from1.5meter high free fall test12years laterAPVCanti-corrosion tiles, there were no penetrating holes or cracks, indicating that the impact strength still maintains its original performance.
Conclusion:
(1) After12years of outdoor use, the product's various performances are still quite excellent.
(2) HongboAPVCanti-corrosion tile warranty20years is guaranteed.
03
HongboAPVCanti-corrosion tiles



APVCAnti-corrosion composite corrugated tile
Since 2012, Hongbo APVC anti-corrosion tiles have been upgraded to a four-layer structure, and the weather resistance and corrosion resistance of the surface material (A layer) have been further improved, adding a secondary weather-resistant layer (B layer), thus further ensuring the product's weather resistance and corrosion resistance.
HongboAPVCAnti-corrosion tile cross-section structure

HongboAPVCAnti-corrosion tiles are widely used in high-end factories, steel structure factories, warehouses, farmers' markets, market passages, car sheds, and other high-end roofing materials,especially in factories with corrosive environments such as ceramic factories, chemical plants, dyeing plants, smelters, and fertilizer plants, the effect is particularly significant.
Professional tile making31year
Nationwide toll-free service hotline:400-161-3388

Official subscription number
Long press to identify and follow
Previous
Related News